The Experts below are selected from a list of 294 Experts worldwide ranked by ideXlab platform

Li Cheng - One of the best experts on this subject based on the ideXlab platform.

  • preparation characterization and properties of Starch based wood Adhesive
    Carbohydrate Polymers, 2012
    Co-Authors: Zhenjiong Wang, Zhengbiao Gu, Zhaofeng Li, Yan Hong, Li Cheng
    Abstract:

    A new biodegradable, renewable, environmentally friendly Starch-based wood Adhesive that can be used at room temperature was synthesized by the graft polymerization of vinyl acetate monomer onto waxy corn Starch. Compared with the blend of commercial PVAc/gelatinized Starch, the shear strength of grafted Starch Adhesive increased by 59.4% in dry state and 321% in wet state, while its water resistance increased by 61.1%. The improved performance of the grafted Starch-based wood Adhesive was supported by its strengthened compatibility with polyvinyl acetate and Starch, based on the results of Fourier-transform infrared, 1H nuclear magnetic resonance, thermogravimetry, and scanning electron microscopy analyses. The most economic monomer feeding ratio was also evaluated using bond characteristics and grafting parameters. A Starch/monomer ratio of 1:1.2 (w/w) was considered as the best ratio in terms of economy.

  • Preparation, characterization and properties of Starch-based wood Adhesive
    Carbohydrate Polymers, 2012
    Co-Authors: Zhe Wang, Zhengbiao Gu, Zhaofeng Li, Yan Hong, Li Cheng
    Abstract:

    A new biodegradable, renewable, environmentally friendly Starch-based wood Adhesive that can be used at room temperature was synthesized by the graft polymerization of vinyl acetate monomer onto waxy corn Starch. Compared with the blend of commercial PVAc/gelatinized Starch, the shear strength of grafted Starch Adhesive increased by 59.4% in dry state and 321% in wet state, while its water resistance increased by 61.1%. The improved performance of the grafted Starch-based wood Adhesive was supported by its strengthened compatibility with polyvinyl acetate and Starch, based on the results of Fourier-transform infrared, 1H nuclear magnetic resonance, thermogravimetry, and scanning electron microscopy analyses. The most economic monomer feeding ratio was also evaluated using bond characteristics and grafting parameters. A Starch/monomer ratio of 1:1.2 (w/w) was considered as the best ratio in terms of economy. ?? 2011 Elsevier Ltd. All rights reserved.

  • Starch based wood Adhesive and preparation method and application thereof
    2011
    Co-Authors: Zhengbiao Gu, Li Cheng, Yan Hong, Hui Wang, Zhaofeng Li
    Abstract:

    The invention provides a Starch-based wood Adhesive and a preparation method and application thereof, and belongs to the technical field of Adhesive. In the invention, a Starch Adhesive for woods with good property is prepared by performing acidolysis and gelatinization on Starch serving as raw materials, grafting, copolymerizing and modifying the Starch by using two monomers of vinylacetate and butyl acrylate under the condition of adding an emulsifier, and adding an accessory ingredient after lowering the temperature. The Adhesive prepared by the preparation method has the advantages of good preservation stability, high bonding strength, milky white and glossy color and the like, and can be applied to decoration of woods and bonding of artificial plates and glued plates.

Zhaofeng Li - One of the best experts on this subject based on the ideXlab platform.

  • preparation characterization and properties of Starch based wood Adhesive
    Carbohydrate Polymers, 2012
    Co-Authors: Zhenjiong Wang, Zhengbiao Gu, Zhaofeng Li, Yan Hong, Li Cheng
    Abstract:

    A new biodegradable, renewable, environmentally friendly Starch-based wood Adhesive that can be used at room temperature was synthesized by the graft polymerization of vinyl acetate monomer onto waxy corn Starch. Compared with the blend of commercial PVAc/gelatinized Starch, the shear strength of grafted Starch Adhesive increased by 59.4% in dry state and 321% in wet state, while its water resistance increased by 61.1%. The improved performance of the grafted Starch-based wood Adhesive was supported by its strengthened compatibility with polyvinyl acetate and Starch, based on the results of Fourier-transform infrared, 1H nuclear magnetic resonance, thermogravimetry, and scanning electron microscopy analyses. The most economic monomer feeding ratio was also evaluated using bond characteristics and grafting parameters. A Starch/monomer ratio of 1:1.2 (w/w) was considered as the best ratio in terms of economy.

  • Preparation, characterization and properties of Starch-based wood Adhesive
    Carbohydrate Polymers, 2012
    Co-Authors: Zhe Wang, Zhengbiao Gu, Zhaofeng Li, Yan Hong, Li Cheng
    Abstract:

    A new biodegradable, renewable, environmentally friendly Starch-based wood Adhesive that can be used at room temperature was synthesized by the graft polymerization of vinyl acetate monomer onto waxy corn Starch. Compared with the blend of commercial PVAc/gelatinized Starch, the shear strength of grafted Starch Adhesive increased by 59.4% in dry state and 321% in wet state, while its water resistance increased by 61.1%. The improved performance of the grafted Starch-based wood Adhesive was supported by its strengthened compatibility with polyvinyl acetate and Starch, based on the results of Fourier-transform infrared, 1H nuclear magnetic resonance, thermogravimetry, and scanning electron microscopy analyses. The most economic monomer feeding ratio was also evaluated using bond characteristics and grafting parameters. A Starch/monomer ratio of 1:1.2 (w/w) was considered as the best ratio in terms of economy. ?? 2011 Elsevier Ltd. All rights reserved.

  • Starch based wood Adhesive and preparation method and application thereof
    2011
    Co-Authors: Zhengbiao Gu, Li Cheng, Yan Hong, Hui Wang, Zhaofeng Li
    Abstract:

    The invention provides a Starch-based wood Adhesive and a preparation method and application thereof, and belongs to the technical field of Adhesive. In the invention, a Starch Adhesive for woods with good property is prepared by performing acidolysis and gelatinization on Starch serving as raw materials, grafting, copolymerizing and modifying the Starch by using two monomers of vinylacetate and butyl acrylate under the condition of adding an emulsifier, and adding an accessory ingredient after lowering the temperature. The Adhesive prepared by the preparation method has the advantages of good preservation stability, high bonding strength, milky white and glossy color and the like, and can be applied to decoration of woods and bonding of artificial plates and glued plates.

Zhengbiao Gu - One of the best experts on this subject based on the ideXlab platform.

  • preparation characterization and properties of Starch based wood Adhesive
    Carbohydrate Polymers, 2012
    Co-Authors: Zhenjiong Wang, Zhengbiao Gu, Zhaofeng Li, Yan Hong, Li Cheng
    Abstract:

    A new biodegradable, renewable, environmentally friendly Starch-based wood Adhesive that can be used at room temperature was synthesized by the graft polymerization of vinyl acetate monomer onto waxy corn Starch. Compared with the blend of commercial PVAc/gelatinized Starch, the shear strength of grafted Starch Adhesive increased by 59.4% in dry state and 321% in wet state, while its water resistance increased by 61.1%. The improved performance of the grafted Starch-based wood Adhesive was supported by its strengthened compatibility with polyvinyl acetate and Starch, based on the results of Fourier-transform infrared, 1H nuclear magnetic resonance, thermogravimetry, and scanning electron microscopy analyses. The most economic monomer feeding ratio was also evaluated using bond characteristics and grafting parameters. A Starch/monomer ratio of 1:1.2 (w/w) was considered as the best ratio in terms of economy.

  • Preparation, characterization and properties of Starch-based wood Adhesive
    Carbohydrate Polymers, 2012
    Co-Authors: Zhe Wang, Zhengbiao Gu, Zhaofeng Li, Yan Hong, Li Cheng
    Abstract:

    A new biodegradable, renewable, environmentally friendly Starch-based wood Adhesive that can be used at room temperature was synthesized by the graft polymerization of vinyl acetate monomer onto waxy corn Starch. Compared with the blend of commercial PVAc/gelatinized Starch, the shear strength of grafted Starch Adhesive increased by 59.4% in dry state and 321% in wet state, while its water resistance increased by 61.1%. The improved performance of the grafted Starch-based wood Adhesive was supported by its strengthened compatibility with polyvinyl acetate and Starch, based on the results of Fourier-transform infrared, 1H nuclear magnetic resonance, thermogravimetry, and scanning electron microscopy analyses. The most economic monomer feeding ratio was also evaluated using bond characteristics and grafting parameters. A Starch/monomer ratio of 1:1.2 (w/w) was considered as the best ratio in terms of economy. ?? 2011 Elsevier Ltd. All rights reserved.

  • Starch based wood Adhesive and preparation method and application thereof
    2011
    Co-Authors: Zhengbiao Gu, Li Cheng, Yan Hong, Hui Wang, Zhaofeng Li
    Abstract:

    The invention provides a Starch-based wood Adhesive and a preparation method and application thereof, and belongs to the technical field of Adhesive. In the invention, a Starch Adhesive for woods with good property is prepared by performing acidolysis and gelatinization on Starch serving as raw materials, grafting, copolymerizing and modifying the Starch by using two monomers of vinylacetate and butyl acrylate under the condition of adding an emulsifier, and adding an accessory ingredient after lowering the temperature. The Adhesive prepared by the preparation method has the advantages of good preservation stability, high bonding strength, milky white and glossy color and the like, and can be applied to decoration of woods and bonding of artificial plates and glued plates.

Yan Hong - One of the best experts on this subject based on the ideXlab platform.

  • preparation characterization and properties of Starch based wood Adhesive
    Carbohydrate Polymers, 2012
    Co-Authors: Zhenjiong Wang, Zhengbiao Gu, Zhaofeng Li, Yan Hong, Li Cheng
    Abstract:

    A new biodegradable, renewable, environmentally friendly Starch-based wood Adhesive that can be used at room temperature was synthesized by the graft polymerization of vinyl acetate monomer onto waxy corn Starch. Compared with the blend of commercial PVAc/gelatinized Starch, the shear strength of grafted Starch Adhesive increased by 59.4% in dry state and 321% in wet state, while its water resistance increased by 61.1%. The improved performance of the grafted Starch-based wood Adhesive was supported by its strengthened compatibility with polyvinyl acetate and Starch, based on the results of Fourier-transform infrared, 1H nuclear magnetic resonance, thermogravimetry, and scanning electron microscopy analyses. The most economic monomer feeding ratio was also evaluated using bond characteristics and grafting parameters. A Starch/monomer ratio of 1:1.2 (w/w) was considered as the best ratio in terms of economy.

  • Preparation, characterization and properties of Starch-based wood Adhesive
    Carbohydrate Polymers, 2012
    Co-Authors: Zhe Wang, Zhengbiao Gu, Zhaofeng Li, Yan Hong, Li Cheng
    Abstract:

    A new biodegradable, renewable, environmentally friendly Starch-based wood Adhesive that can be used at room temperature was synthesized by the graft polymerization of vinyl acetate monomer onto waxy corn Starch. Compared with the blend of commercial PVAc/gelatinized Starch, the shear strength of grafted Starch Adhesive increased by 59.4% in dry state and 321% in wet state, while its water resistance increased by 61.1%. The improved performance of the grafted Starch-based wood Adhesive was supported by its strengthened compatibility with polyvinyl acetate and Starch, based on the results of Fourier-transform infrared, 1H nuclear magnetic resonance, thermogravimetry, and scanning electron microscopy analyses. The most economic monomer feeding ratio was also evaluated using bond characteristics and grafting parameters. A Starch/monomer ratio of 1:1.2 (w/w) was considered as the best ratio in terms of economy. ?? 2011 Elsevier Ltd. All rights reserved.

  • Starch based wood Adhesive and preparation method and application thereof
    2011
    Co-Authors: Zhengbiao Gu, Li Cheng, Yan Hong, Hui Wang, Zhaofeng Li
    Abstract:

    The invention provides a Starch-based wood Adhesive and a preparation method and application thereof, and belongs to the technical field of Adhesive. In the invention, a Starch Adhesive for woods with good property is prepared by performing acidolysis and gelatinization on Starch serving as raw materials, grafting, copolymerizing and modifying the Starch by using two monomers of vinylacetate and butyl acrylate under the condition of adding an emulsifier, and adding an accessory ingredient after lowering the temperature. The Adhesive prepared by the preparation method has the advantages of good preservation stability, high bonding strength, milky white and glossy color and the like, and can be applied to decoration of woods and bonding of artificial plates and glued plates.

Zhenjiong Wang - One of the best experts on this subject based on the ideXlab platform.

  • preparation characterization and properties of Starch based wood Adhesive
    Carbohydrate Polymers, 2012
    Co-Authors: Zhenjiong Wang, Zhengbiao Gu, Zhaofeng Li, Yan Hong, Li Cheng
    Abstract:

    A new biodegradable, renewable, environmentally friendly Starch-based wood Adhesive that can be used at room temperature was synthesized by the graft polymerization of vinyl acetate monomer onto waxy corn Starch. Compared with the blend of commercial PVAc/gelatinized Starch, the shear strength of grafted Starch Adhesive increased by 59.4% in dry state and 321% in wet state, while its water resistance increased by 61.1%. The improved performance of the grafted Starch-based wood Adhesive was supported by its strengthened compatibility with polyvinyl acetate and Starch, based on the results of Fourier-transform infrared, 1H nuclear magnetic resonance, thermogravimetry, and scanning electron microscopy analyses. The most economic monomer feeding ratio was also evaluated using bond characteristics and grafting parameters. A Starch/monomer ratio of 1:1.2 (w/w) was considered as the best ratio in terms of economy.